Description
Best Sialon Extrusion dies
Sialon long-life extrusion dies provide performance cost advantages to the non-ferrous foundry industry. If you have any question, please feel free to contact us. Thanks for being with us.
A new generation of Sialons with an increased impact fracture toughness up to 1.400° Celsius / 2624° Fahrenheit.
A new generation of Sintered Silicon Carbide with superior or equal performance to HEXOLOY® | For use in molten metals up to 1900 °Celsius
Home » Request for Quotation Shop » Sialon Extrusion dies
Sialon long-life extrusion dies provide performance cost advantages to the non-ferrous foundry industry. If you have any question, please feel free to contact us. Thanks for being with us.
Material data sheet | Sialon (Si3Al3O3N5) | ||||
Typical Sialon grades | NVD-001 | NVD-002 | NVD-003 | NVD-004 | |
Bulk Density | g/cm3 | 3.2 | 3.1 | 3.3 | 3.2 |
Water Absorption | % | 0 | 0 | 0 | 0 |
Flexural Strength | MPa | 580 | 900 | 1,020 | 790 |
Vickers Hardness HV1 | GPa | 13.9 | 12.7 | 15.0 | 13.8 |
Fracture Toughness (SEPB) | MPam1/2 | 4 ~ 5 | 6 ~ 7 | 7 | 6 ~ 7 |
Young’s Modulus of Elasticity | GPa | 290 | 270 | 300 | 290 |
Poisson’s Ratio | – | 0.28 | 0.28 | 0.28 | 0.28 |
Coefficient of Linear Thermal (40 – 800 °C)
Expansion |
×10-6/℃ | 3.2 | 3.4 | 3.3 | 3.5 |
Thermal Conductivity (20℃) | W/(m・k) | 25 | 23 | 27 | 54 |
Specific Heat | J/(g・k) | 0.64 | 0.66 | 0.65 | 0.66 |
Heat Shock Resistance | ℃ | 550 | 800 | 800 | 900 |
Volume Resistivity (20℃) | Ω・cm | >1014 | >1014 | >1014 | >1014 |
Please visit our brochure page to get a free download!
We ship usually within 4 weeks
In molten aluminium baths
Since 1986
Invalid number
Sweden / Sverige
+(46) 31 754 0790
Invalid number
Denmark
+(45) 35 15 8085
Invalid number
United Kingdom
+(44) 20 7660 2162
Invalid number
USA/Canada Tollfree
+ 1 (833) 709-1399
Invalid number
©2024 All Rights Reserved. Sialon Ceramics Sweden AB